Configuration and Erosion Mechanisms of Blast Furnace Refractories
News

Configuration and Erosion Mechanisms of Blast Furnace Refractories

2026-10-16

NO. 1 Refractory Lining Configuration for Blast Furnaces

As blast furnaces evolve toward larger scales, higher efficiency, and longer service lives, the refractories used in them have undergone significant changes; new, high-efficiency, and long-lasting refractory materials are increasingly being adopted and applied.
01 Refractories for the Upper and Middle Sections of the Furnace Shaft
The upper and middle sections of the furnace shaft operate at relatively lower temperatures, where there is no slag formation or risk of slag corrosion. However, the lining in these areas must withstand abrasion from solid materials, erosion from high-temperature gas flows, and a certain degree of chemical attack. Consequently, the linings in the upper and middle sections typically consist of high-quality, low-porosity fireclay bricks or high-alumina bricks. In some cases, phosphate-bonded fireclay bricks or sillimanite-based refractory bricks—which offer superior spalling resistance and wear resistance—are used.

02 Refractory Materials for the Lower Blast Furnace Shaft
There have long been two competing schools of thought regarding the selection of refractory materials for the lower section of a blast furnace shaft. The "refractories-focused" school posits that damage in this region is primarily driven by high-temperature abrasion and chemical erosion; consequently, they advocate for the use of high-quality, low-thermal-conductivity, high-strength, and erosion-resistant materials—such as corundum-based or bonded silicon carbide (SiC) bricks. In contrast, the "thermodynamics-focused" school argues that temperature fluctuations are the primary cause of lining degradation. They recommend employing highly efficient cooling systems in conjunction with high-thermal-conductivity materials—such as carbon or graphite-based products—for the furnace lining. This approach lowers the temperature at the hot face of the lining, thereby enhancing resistance to severe thermal shock, while simultaneously facilitating the formation of a protective "slag skull" (a solidified layer of slag) that extends the service life of the refractory lining.

03 Refractory Materials for the Blast Furnace Bosh and Bosh Parallel
The bosh, bosh parallel, and the lower section of the furnace shaft constitute a critical zone within a blast furnace where materials undergo complex chemical reactions. This area is subjected to mechanical abrasion from the furnace burden, erosion by hot gas streams, chemical attack by harmful elements, and corrosion by molten materials. Consequently, the refractory materials employed in these zones must exhibit excellent resistance to chemical corrosion, oxidation, and alkali attack, as well as high thermal conductivity, superior thermal shock resistance, and high wear resistance.

04 Refractories for the Blast Furnace Hearth and Bottom
Refractories used in the blast furnace hearth and bottom are subjected not only to high temperatures but also to chemical erosion by slag and iron, as well as the erosive scouring action of molten iron; furthermore, they face severe attack from alkalis and zinc. Consequently, these refractories must possess excellent resistance to erosion, permeability, and alkali attack. Currently, blast furnace hearths and bottoms worldwide primarily utilize one of two structural designs: an all-carbon structure or a composite carbon-ceramic structure.

The all-carbon structure relies on the use of semi-graphitic carbon blocks with high thermal conductivity to rapidly transfer heat to the cooling system, thereby achieving thermal equilibrium. This process lowers the temperature at the working face and promotes the formation of a protective slag layer; it also shifts the 800°C isotherm outward beyond the carbon bricks, ensuring the safety and longevity of the hearth system.

While the composite carbon-ceramic design shares the principles of the all-carbon structure, it incorporates a "ceramic cup"—made from ceramic materials with superior resistance to erosion, scouring, and thermal shock—to isolate the carbon-based hearth lining from the molten iron and other mixtures. This barrier effectively prevents molten iron from eroding the carbon lining for an extended period, thereby ensuring the hearth system operates safely, efficiently, and with a long service life.

Zhengzhou ShengKun Refractory Co., Ltd. is a specialized manufacturer of refractory materials for industry furnaces.
If you currently have any requirements, please let me know; I would be happy to calculate a highly competitive price for your reference.

Email address : sales@skrefractory.com

2021_06_01_18_48_IMG_8818_副本.jpg

NO. 2 Erosion Mechanisms of Refractory Materials in Blast Furnaces
As materials descend through a blast furnace, continuous heat exchange occurs, creating variations in temperature, pressure, and atmosphere within the furnace. Consequently, the mechanisms of degradation for refractory materials differ depending on their location. The erosion mechanisms affecting blast furnace linings—and their approximate relative contributions—are as follows: alkali metal attack (40%); oxidation by gases such as CO and H₂O (20%); mechanical wear (10%); issues related to poor thermal conductivity (10%); thermal shock damage (15%); and slag erosion (5%). In reality, the degradation of a blast furnace lining is the result of the combined effects of several such destructive factors.

The lining in the upper section of the furnace shaft experiences the most severe mechanical wear, while the bosh, the furnace waist, and the lower section of the shaft suffer the most intense erosion. In the bosh, the furnace waist, and the middle-to-lower sections of the shaft, the lining is primarily subjected to three types of stress: erosion/scouring by high-temperature gases and molten iron; high heat flux and thermal shock; and damage caused by alkali metals and zinc. Among these, the destructive impact of alkali metals and zinc is the most significant, followed by thermal shock and mechanical wear, while slag erosion plays the smallest role.

In recent years, in an effort to increase the utilization coefficient of blast furnaces, the temperature of molten iron has been raised. This has led to more severe degradation of the refractory lining in the hearth—particularly in the taphole area and the regions below it—which has become a critical factor limiting the service life of blast furnaces.

Erosion in the center of the furnace bottom often results in a "pot-bottom" (concave) profile, while erosion in the hearth typically takes on an "elephant-foot" shape. This abnormal erosion is driven by several factors: first, the penetration and circulation of molten iron cause structural changes and mechanical wear in the carbon bricks. Furthermore, alkali metals—along with gases—can penetrate the carbon bricks, reaching the 800°C isotherm. Here, they react to form carbonate deposits within the brick structure, which subsequently react with the carbon itself. As production continues, these ongoing reactions lead to the formation of a brittle layer. The chemical reactions are as follows:

2K(g) + 2CO2(g) = K2CO3(l) + CO(g) (1)

K2CO3(l) + 2C(s) = K(g) + 3CO(g) (2)

Consequently, when selecting refractory materials for the hearth and furnace bottom, it is essential to choose or develop materials with superior overall performance based on these mechanisms. Additionally, a composite hearth structure should be considered: utilizing dense, high-performance refractories for the working layer to resist molten iron penetration and alkali attack, while employing materials with high thermal conductivity near the cooling staves.